원문정보
The effect of the gold based bonding agents on the bond between Ni-Cr alloys and ceramic restorations
초록
영어
The success of a porcelain fused to metal (PFM) restoration depends upon the quality of the
porcelain-metal bond. The adhesion between metal substructure and dental porcelain is related to the diffusion of oxygen to the reaction layer formed on cast-metal surface during firing.
The purposed of this investigation was to study the effects of gold based bonding agent on Ni-Cr
alloy-ceramic adhesion between porcelain matrix, gold based bonding agent and metal substructure interface. gold based bonding agent have been applied as an intermediate layer between a metal substructure and a ceramic coating. gold based bonding agent(Aurofilm NP, Metalor, Swiss) was applied on Ni-Cr alloy surface by four method. Surfaces only air abraded with 110ß≠ Al2O3 particles were used as control. metal ceramic adhesion was evaluated by a biaxial flexure test(N=5) and volume fraction of adherent porcelain was determined by SEM/EDS analysis. Result of this study suggest that the layering sequence of gold based bonding agent is very important and can improve porcelain adherence to PFM.
목차
Ⅰ. 서론
Ⅱ. 실험 재료 및 방법
1. 실험 재료
2. 연구 방법
Ⅲ. 실험 결과 및 고찰
1. SEM photographs
2. EDS Analysis
Ⅳ. 결론