Mechanical Characteristics of Post Weld Heat Treatment for Friction Welding of SM45C-STKM13B Hollow Shaft
초록
영어
In this study, SM45C-STKM13B hollow shaft of different thickness was joined by friction welding. After friction welding, we treated to specimen of annealing(post-weld heat treatment). The specimens were tested as-welded and post-weld heat treatment(PWHT). The mechanical properties including tensile test and vickers micro-hardness were examined. And then, the mechanical properties were compared for as-welded and PWHT in SM45C to STKM13B. Microstructure of joining part were examined in the weld interface and weld region and heat affected zone and base metal of weld parts.