A Study on the Metal-Ceramic Bond Strength of CAD/CAM Metal Disk Alloy and Casting Alloy
초록
영어
Purpose: The purpose of this study was to evaluate bond strength of Metal Disk alloy and casting alloy. Methods: Metal specimens were divided into 4 groups for each alloy. Three point flexural test were used to measure the bond strength of CAD/CAM metal alloy and casting alloy. Statistical analysis was done using the Statistical Package for Social Sciences version 19.0 for Windows. As for the analysis methods, the study used Kruskal-Wallis test. Results: The average bonding strengths of Group 1 to porcelain was 36.7±9.90 MPa, Group 2 to porcelain was 37.68±4.51 MPa, Group 3 to porcelain was 36.43±6.57 MPa, Group 4 to porcelain was 42.88±6.81 MPa, Each group was not significantly different. Conclusion: Bond strength of Casting alloy is equal to or higher than bond strength of CAD/CAM Metal Disk alloy. Alloy clinical bond strength is 25 MPa, So CAD/CAM Metal Disk alloy can be used as dental material.
목차
Ⅰ. 서론
Ⅱ. 연구 방법
1. 연구 재료
2. 금속시편 제작
3. 도재의 소성
4. 3점 굴곡강도 측정
5. 통계 처리
Ⅲ. 결과
Ⅳ. 고찰
Ⅴ. 결론
REFERENCES