earticle

논문검색

인공풍화암을 이용한 강화제의 적용실험 연구

원문정보

An Experimental Application of Consolidants Using Artificially Weathered Stones

이재만, 이명성, 김재환, 이미혜, 박성미

피인용수 : 0(자료제공 : 네이버학술정보)

초록

영어

This study was to assess the effect of consolidation for intension measures of stone cultural heritage using artificially weathered stones. We have prepared four kinds of stones (Gyeongju Namsan Granite, Iksan Granite, Yeongyang Sandstone, Jeongseon Marble), and manufactured fresh, weathered and highly weathered stone samples by thermal shock for each rock type. The samples were treated with three consolidants (Wacker OH 100, Remmers KSE 300, 1T1G) by three methods {immersion, capillary rise (partial immersion), spray}, and tested for weight, porosity, ultrasonic velocity, Equotip hardness and color before and after treatment. As a result, the effect of consolidation was widely influenced by porosity and treatment methods. Wacker OH 100 was shown the highest consolidation effect in almost every stone sample.

한국어

이 연구에서는 석조문화재의 재질과 풍화 상태에 따른 강화처리 방안을 도출하기 위해 인공적으로 풍화시킨 암석을 이용하여 강화처리의 효과를 평가하였다. 시료는 2종의 화강암(경주 남산, 익산)과 영양 사암 및 정선 대리암을 사용하였으며, 미처리 및 400℃, 600℃에서 열처리하여 신선암, 중간풍화암, 심한풍화암의 세 등급으로 분류하였다. 3종의 강화제(Wacker OH 100, Remmers KSE 300, 1T1G)를 함침, 모세관 흡수(부분 침적), 분무법으로 적용하고 처리 전후의 중량, 공극률, 초음파속도, 에코팁 경도 및 색도 변화를 비교하였다. 실험 결과, 강화 효과는 암석의 풍화 상태와 처리 방법에 의해 크게 영향을 받으며, 대부분의 조건에서 Wacker OH 100의 효과가 큰 것으로 나타났다.

목차

초록
 ABSTRACT
 1. 서론
 2. 연구 방법
  2.1. 시료 제작
  2.2. 강화제 선정
  2.3. 강화처리 및 양생
  2.4. 강화제 성능평가
 3. 결과 및 해석
  3.1. 중량과 공극률의 변화
  3.2. 초음파속도의 변화
  3.3. 에코팁 경도의 변화
  3.4. 표면 색변화
 4. 고찰 및 결론
 사사
 참고문헌

저자정보

  • 이재만 Jae Man Lee. 국립문화재연구소 보존과학연구실
  • 이명성 Myeong Seong Lee. 국립문화재연구소 보존과학연구실
  • 김재환 Jae Hwan Kim. 국립문화재연구소 보존과학연구실
  • 이미혜 Mi Hye Lee. 국립문화재연구소 보존과학연구실
  • 박성미 Sung Mi Park. 국립문화재연구소 보존과학연구실