원문정보
초록
영어
A inorganic powder EL lamp was made by screen printing technique with phosphor ink and dielectric ink. The thickness change of a phosphor ink layer and a dielectric ink layer were not influenced on dielectric content, but rely on phosphor size and vehicle. Once finishing screen printing technique with phosphor ink and dielectric ink, and its surface has been printed again before not drying of phosphor ink and dielectric ink. Then phosphor ink and dielectric ink were not transferred. The electric capacity of inorganic powder EL lamp was more influenced on dielectric content than the thickness of dielectric ink layer, and it was more dependent on the thickness of phosphor ink layer than the thickness of dielectric ink layer.
목차
1. 서론
2. 실험
2-1. 실험 기자재
2-2. 실험 방법
3. 결과 및 고찰
3-1. 스크린 인쇄 기법에 따른 형광층 및 유전층의 두께 변화
3-2. 형광층 및 유전층의 두께에 따른 정전용량의 변화
4. 결론
참고 문헌