영어

Stereo-Microscope observation, ultrasonic velocity, shore hardness and standard color measurement performed for studies of physical characterization of Namsan granite after treated with consolidants. The consolidants used in experiment are 35wt% Silicate Nonparticle/100%1T1G (Nonparticle), 3%POSS-SO1455/97%1T1G(3%POSS1455), POSS-SO1458/97%1T1G (3%POSS1458), 3%7nm/97%1T1G(3%7nm), 3%16nm/97%1T1G(3%16nm), 3% 40nm/ 97%1T1G(3%40nm) develop with Sejong university, and Wacker Silres BS OH-100, Unil Sandsteinfestiger OH-100. The color of rock surface is darker than original one but similar to original samples with time, and ultrasonic velocity and shore hardness increased with after consolidant treatment.

한국어

경주 남산화강암에 대한 강화제 처리 전후의 물리적 특성변화 연구를 위하여 강화제 처리 한 후 쌍안실체현미경 관찰, 초음파속도, 쇼어경도, 색도측정 등을 실시하였다. 실험에 사용한 강화제는 세종대학교에서 개발한 6종류 35wt% Silicate Nonparticle/100%1T1G (Nonparticle), 3%POSS-SO1455/97%1T1G (3%POSS1455), POSS-SO1458/97%1T1G (3%POSS1458), 3%7nm/97%1T1G (3%7nm), 3%16nm/97%1T1G(3%16nm), 3%40nm/97%1T1G(3%40nm)와 상품 화된 제품인 2개 Wacker사의 Silres BS OH-100, Kulba사의 Unil Sandsteinfestiger OH-100으로 총 8가지 종류이다. 강화제 처리후 암석의 표면색깔은 강화제의 종류에 따라 약간의 차이는 있으나 대부분 어두워졌으며 시간이 지남에 따라 원암과 유사한 색깔을 나타낸다. 강화제 처리 후 초음파속도와 쇼어경도는 증가하였다.

목차

초록
 ABSTRACT
 1. 서언
 2. 연구방법
 3. 연구 결과
  3.1. 경주 남산화강암의 암석학적 특성
  3.2. 강화제 처리 후 시료의 표면 특성
  3.3 색도 측정결과
  3.4. 초음파 속도측정
  3.5. 반발강도(shore 경도) 측정 결과
 4. 결언
 참고문헌

저자정보

  • 김성호 Sung Ho Kim. 지구환경과학과
  • 원종옥 Jongok Won. 세종대학교
  • 강용수 Young Soo Kang. 한양대학교
  • 장윤득 Yun Deuk Jang. 경북대학교
  • 김사덕 Sa Dug Kim. 국립문화재연구소
  • 김정진 Jeong Jin Kim. 안동대학교

참고문헌

자료제공 : 네이버학술정보

    함께 이용한 논문

      ※ 기관로그인 시 무료 이용이 가능합니다.

      • 4,300원

      0개의 논문이 장바구니에 담겼습니다.