This study is to test the possibility of applying the low-molecular weighted waste cellulase, which is produced in the process of cellulase production, to paper making. After experimenting on high-crystallized non-wood fibers with beating catalyst. I got the result that the condition for the optimal effect is temperature 40~60℃, the time 90min to 120min, pH 5.0 to 6.0, the enzyme contents 0.3% and that the effect of beating such as slight reduction of fiver viscosity, increase of water retention value(WRV) and shortening of fiber length was increased with waste cellulase. Through this process, the density, folding endurance, tensile strength and burst strength of paper was remarkably increased, which is inferred to result from the increased flexibility of fiber by individual characteristics of non-wood fiber, which was high-crystallized by penetrated low-molecular weight cellulases in the fiber.
목차
1. 서론
2. 재료 및 방법
2.1. 공시재료
2.2. 실험방법
3. 결과 및 고찰
3.1. 최적 처리조건 선정
3.2. 효소처리 조건별 고해도 변화
3.3. 효소처리에 의한 섬유의 특성변화
3.4. 종이의 강도변화
3.5. 전자현미경 관찰
4. 결론
참고문헌