초록 열기/닫기 버튼

In this experiment, we selected "Tangshan bone china" 10.5-inch white porcelain flat plate produced by five differententerprises as experimental samples to study the erosion of bone porcelain enamel by different kinds of acidic reagents atdifferent temperatures. The specific experimental process was as follows: at different temperatures, 20% hydrochloric acid,30% sulfuric acid, 100 g/L citric acid and 10% acetic acid were used to continuously erode the sample glaze for 10h, and thewhiteness and 45º mirror direction gloss were measured every 2h. The results show that different acidic reagents at differenttemperatures have significant differences in the erosion characteristics and strength of bone porcelain glaze, and the corrosionresistance of products from different enterprises also have significant differences.